Abstract

The formation of an Fe-Al intermetallic compound film on carbon steel by shot lining and heat treatment was investigated. In the experiment, a centrifugal-type peening machine with an electrical heater was employed. The shot medium was high-carbon cast steel. The substrate was a commercial carbon steel, and the sheet was commercially available pure aluminum. The shot lining process of carbon steel with an aluminum sheet was carried out at 300 °C in air using a peening machine. Heat treatment was performed at diffusion temperatures from 600 to 1050 °C in vacuum. The lined substrates exhibited a harder layer of Al-rich intermetallics, such as Fe2Al5, in the diffusion temperature range of 650 to 900 °C. When the temperature of the lined substrates was more than 930 °C, the surface was covered with thicker and highly anticorrosive layers of Fe-rich intermetallics, such as FeAl and Fe3Al. We found that the present method could be used for the formation of functional films on carbon steel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.