Abstract

AbstractThe formation and microstructure of quasicrystals in suction cast Al‐6 wt.% Mn‐2 wt.% TM (TM = Ni, Fe) alloys were investigated by transmission electron microscopy, scanning electron microscopy, energy dispersive spectrometry, and X‐ray diffraction. The suction cast Al‐6 wt.% Mn‐2 wt.% Ni alloy consists of a single decagonal phase of Al56Mn11Ni2, whereas the Al‐6 wt.% Mn alloy with 2 wt.% iron addition comprises a primitive icosahedral phase and a decagonal phase of Al40Mn7Fe2. Thus, the addition of nickel or iron favors quasicrystal formation in the suction cast Al‐6 wt.% Mn alloys. Based on a 4 : 1 matching ratio of aluminum atoms to heavier atoms, the approximate electron to atom ratio is 1.85 in two decagonal phases of Al56Mn11Ni2 and Al40Mn7Fe2. Various morphologies of quasicrystals with a size of more than 5 μm were observed in the microstructure of suction cast Al‐6 wt.% Mn‐2 wt.% TM (TM = Ni, Fe) alloys. The decagonal Al40Mn7Fe2 phase nucleates epitaxially and grows on the icosahedral phase.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.