To obtain high quality CsLiB 6O 10 (CLBO) crystal, we used NaF as flux to grow CLBO crystals for the first time. The solubility of CLBO showed that the favorable mol concentration of CLBO in the NaF flux system was in the range of 65–85%. The viscosity of solutions was investigated. Using the top-seeded solution growth (TSSG) method, a CsLiB 6O 10 (CLBO) crystal with the dimensions of 54×51×32 mm 3 was grown from the NaF flux system. A 5×5×5 mm 3 crystal sample cut from the grown CLBO crystal was etched by an etchant that consisted of 15 ml glycerol and 15 ml water at room temperature, for comparison with another CLBO crystal sample got from the self-flux system was used. From the surface etching patterns, it was indicated that CLBO crystal grown from NaF flux system may be more stable than that from self-flux system.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.