Abstract

Undoped and Ce-doped GdTaO4 single crystals with different Ce concentration were grown by the floating zone method. By X-ray diffraction analysis, we confirmed all the grown crystals do not have any impurity phases. In X-ray induced scintillation spectra, the undoped sample shows a broad emission band around 300–700 nm, and the decay time of this emission is around 500 ns In Ce-doped samples, emissions are observed around 400–700 nm, and the decay time constants are around 50 ns which is a typical value of the 5d-4f transitions of Ce3+. In order to reveal the detailed scintillating behaviors, we measured the temperature dependence of X-ray induced scintillation spectra and revealed the energy transfer mechanisms between two different excited states of luminescent centers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.