Abstract
ABSTRACTIn this work, the poled PVDF with metal coating was prepared. The microscopy characterization and crystalline phase were studied. The piezoresponse force microscope (PFM) test, nanoindentation and nanoscratch tests were carried out. The focus of this work is on the morphology, local piezoelectric deformation, and the key properties of PVDF sheet with coating, such as the hardness, roughness, critical load and so on. The aim is to determine surface characteristic, ferroelectric domain and mechanical properties of PVDF sheet and can avoid the unfavorable effect that the sample served as an actuator broke during the bending deformation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.