Abstract
Abstract Phase transitions in the solid solution Sr χ(Na 0.5Bi 0.5)l-χTiO3 have been studied by dielectric, pyroelectric and D-E characteristic measurements. An intermediate antiferroelectric phase has been observed in the composition range of 0 ⩽ χ ⩽ 0.5 of this system. These compositions undergo a ferroelectric-antiferroelectric-paraelectric sequence of transitions at elevated temperatures. The antiferroelectric phase transition temperature and Curie point decrease monotonically with increasing SrTiO3 concentration.