Abstract

The success of metal injection moulding (MIM) process is significantly influenced by the homogeneity level of the powder-binder mixture (feedstock). This paper highlights some initial characterization of the feedstock containing elemental Ni and Ti powders mixture, (50.8 at.% Ni/ 49.2 at.% Ti) mixed with Palm stearin-based binder system. The feedstock was prepared using an internal mixer, HAAKE Rheomix at a temperature of 160°C for 2 hours. The feedstock was then characterized by Differential Scanning Calorimetry (DSC), Thermogravimetric (TGA), Scanning Electron Microscopy (SEM) and Capillary Rheometer. All the results obtained were analyzed and discussed for further injection moulding process.