Abstract

AbstractBy fast heating the nano‐sized Al2O3 and carbon black mixtures at 50°C/min to 1750°C for 30–120 min, single‐phase AlON powders were successfully obtained by a fast one‐step carbothermal reduction and nitridation (CRN) method. The AlON ceramics pressureless sintered at 1880°C for 150 min by these powders show high transmittances up to 83%–84%, which indicates that the proposed fast one‐step CRN method is an effective and efficient way with strong robustness to synthesize single‐phase AlON powder for highly transparent AlON ceramics. It was found that α‐Al2O3 particles do not have enough time to aggregate and coalesce during heating due to the tremendously shortened heating span, which significantly inhibited particle coarsening until the formation of AlON starts. The fast‐formed AlON further inhibits the coarsening of α‐Al2O3 during dwelling. Consequently, single‐phase AlON powder of small primary particles can be obtained after 30 min dwelling at 1750°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.