In general, fly ash is often used as a binder in geopolymer mixture. In this paper, seven samples of fly ash were collected from five Indonesian power plants. The variation of fly ash may depend upon many factors. However, there is no standardization of fly ash used for geopolymer binder. This experiment was conducted to study and categorize fly ashes both by assessing their physical and chemical characters. All fly ashes were activated with alkali activator to prepare geopolymer paste. Ratio of fly ash to the alkali activator was kept constant at 65 : 35. Compression test was conducted at three, seven, 14, 21, 28, and 56 days to identify the strength development of each sample. The result revealed that the content of CaO in fly ash affected the setting time and early strength development. In three days paste with CaO content more than 20% gain 54% of its 28-day strength. It is caused by both hydration and polymerization reactions. A range of Si to Al ratio contributed to the strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.