Abstract
The hematite {001} possessed more adsorption sites, more positive redox potential, and higher conductivity than {100}, resulting that the dissimilatory iron reduction rate of hematite {001} by S. putrefaciens CN-32 was easier than that of {100}.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.