Abstract

This paper presents the fabrication of intermediate x-ray mask for deep x-ray lithography. In order to have working mask with absorbers thickness larger than 10 μm, the intermediate mask should have absorbers of 0.7 μm in thickness. To demonstrate intermediate mask fabrication, x-ray zone plates are fabricated on the 1.2 μm low-stress silicon-rich silicon nitride (SiNx) membrane with the tri-layer Chromium-Tungsten-Chromium (Cr–W–Cr) as the x-ray absorbers. The chromium layers both 200 angstroms are used as adhesion and for stress relief. The SiNx film is deposited with low pressure chemical vapor deposition (LPCVD) and the free standing membrane are formed by KOH silicon backside etching. With the e-beam lithography and reactive ion etching, width of 0.8 μm of outmost zone of the x-ray zone plates has been achieved on the membrane. The scanning electron microscopy (SEM) images of the x-ray zone plates and pictures of intermediate masks are demonstrated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.