Abstract
Nanocrystallite ceria-doped scandia-stabilized zirconia (1Ce10ScSZ) powders are prepared using a combination of co-precipitation and hydrothermal treatments. Power density of 1.0 W cm(-2) is obtained at 1.6 A cm(-2) and 800 °C due to the drastic reduction of ohmic and polarization resistance in the SOFC cell.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.