α-MnO2 nanowires (NWs) prepared by hydrothermal method are characterized using XRD and FT-IR. The crystallite size, surface area of NWs increases, whereas dislocation density and band gap decreases with an increase in oxidizer molarity. The band gap decreases from 2.55 to 1.27eV. The above observations correlate well with the enhanced catalytic activity of MnO2 NWs for degradation of azo dye reactive black 5 (RB5). About 70% of the dye were successfully removed in 60min using 20mg of MnO2 NWs in the presence of 6mL of H2O2. MnO2 NWs show a good reusability, suggesting it as an effective and recyclable catalyst.