On the basis of the surface grinding-hardening test, the influence of depth of cut and original microstructure on the hardened layer depth, microstructure and micro-hardness of the hardened layer were studied. The results show that the hardened layer is consisted of completely hardened region and transitional region. The completely hardened region is composed of mixed martensite, residual austerities and a little carbide. There were no remarkable effects of the depth of cut and original structure on the martensite configuration and micro-hardness value in completely hardened region. The micro-hardness value of the completely hardened region can be up to 750-780HV. However, microstructure of the transitional region varies with different original structure. When the depth of cut or uniformity of original structure increase, the hardened layer depth increases accordingly. Thus in practical production, it should adopt large depth of cut or use the original structure with quenched and tempered to increase the hardened layer depth.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.