Abstract

The tests of the glass exposed to radiant heat and the localized fires were conducted to clarify the behavior of the float plate glass in the early of fire phase. The main results are as follows. 1. The mean temperature difference between the part exposed to fires and the part shaded by window frame is affected by the size of the glass and the speed of heating. 2. The float plate glass put the safety film has the performance holding the broken piece during the phase when the early cracks occur. The pieces of glass fall out when the temperature of the glass surface on the film side reaches the critical value.By using these results, the case study for the float plate glass with the safety film faced the atrium was carried out.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.