Abstract

In this study, Austenitic AISI 304L stainless steel was welded with Ferritic AISI430 stainless steel by MIG–welding using welding electrode ER347 and pure Ar and Ar+2%O2 as the shielding gases. The welded samples were polished and dipped into different concentration of HCL solutions of 0.1M, 0.2M, 0.3M and 0.5M concentrations. Weight change of the samples per week in different concentration of HCL solution was noted for 4 weeks and with the help of weight loss, corrosion rate was calculated. The percentage weight loss was observed to be more when welding was done using pure-Ar as a shielding gas compared to Ar+2%O2. Welded samples were also characterized by means of microscopic and electrochemical investigation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.