Abstract

Ceramic Waste partially replaced as a substitute for coarse aggregates in concrete has been investigated. Two types of ceramic waste, namely tiles and flowerpot were used. Concrete mixtures with characteristic strength of 28 days 30 N/mm2 have been prepared using a water/cement ratio of 0.5. The strength of the concrete mixes containing recycled ceramic waste aggregates was compared to conventional concrete. Compressive strength of concrete made from ceramic waste aggregate is studied with 0, 10, 20, 30 and 40% replacement of natural coarse aggregate by ceramic waste aggregate.