Abstract

Aiming to solve the problem of hard to fill duct completely, the reasons are discussed. Water-cement ratio and admixture are the main influence factors to bleeding rate. There is a minimum grout bleeding rate when water-cement ratio is 0.38 and admixtures are added. The best treatment measure to grout leakage is to flushing out the grout and re-grouting via the on-site grouting test.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.