Abstract

Cerium and magnesium strengthened aluminum alloys, or Al-Ce-Mg, is a recently developed alloy family that exhibits good mechanical properties at elevated temperatures (~300 °C). To examine the single-crystal properties of Al-Ce-Mg alloys, nanoindentation experiments are conducted in this study. A crystal plasticity finite element model (CPFEM) with the evolution of geometrically necessary dislocations (GNDs) is applied to simulate the indentation in individual grains. A parametric study is carried out to investigate the sensitivity of each crystal plasticity model parameter to the indentation behavior. The highly sensitive parameters are calibrated by matching the indentation load-depth curves, while the rest parameters are obtained from bulk polycrystal uniaxial tension tests. Overall, satisfactory matching between experiment and simulation is obtained for each individual grain. The calculated hardness, as determined from the experiment, shows the dependence on indent depth, which is captured by the GND model. Furthermore, the effect of grain orientation and neighboring grains to nanoindentation behavior have been discussed with the comparison between the simulation and experiments.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.