Abstract
A new correction method which is appropriate for the evaluation of Young's modulus of crystalline compounds has been examined and established to correct the size effect. Using a nanoindentation test and the established correction method, Young's moduli of primary Si phase, Al–(Fe,Mn)–Si and Al–Ni compound phases in the hypereutectic Al–Si die cast alloys were evaluated to be 182±9, 208±29 and 170±4 GPa respectively. The rule of mixtures for Young's modulus and the area fraction of each phase were applied to evaluate the Young's modulus of aluminium die cast alloys. The Young's modulus calculated by the rule of mixtures is in good agreement with the value obtained by a tensile test. The combination of the rule of mixtures and nanoindentation test is an effective approach to the precise evaluation of the Young's modulus of aluminium die cast alloys having complicated microstructures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.