Abstract
AbstractThis work presents an in‐depth experimental study aimed at assessing the impact of natural weathering on the behavior of high‐density polyethylene (HDPE) bottles. To this end, several analytical techniques were employed, including Fourier transform infrared spectroscopy (FTIR) to examine molecular changes, scanning electron microscopy (SEM) to study morphology, thermogravimetric analysis (TGA) to assess thermal properties, and tensile and compression tests to evaluate mechanical properties. The results obtained reveal significant changes in HDPE exposed to natural weathering. FTIR analysis enabled us to identify that the HDPE bottles had been subjected to an oxidation process initiated by the absorption of solar radiation during natural weathering treatments, while SEM analysis showed the presence of holes resulting from the detachment of material fragments after exposure, TGA analysis confirms the impact of natural exposure time on the decrease in the average molecular weight and chemical degradation of HDPE macromolecules, through a reduction in the initial degradation temperature and the maximum thermodegradation temperature. However, tensile and compressive tests showed a reduction in the mechanical strength of HDPE after exposure to natural conditions, with notable variations depending on environmental conditions, making the material damaged. These results enabled us to calculate the damage caused by three damage laws. These results offer important insights into the mechanisms of HDPE degradation under the influence of natural climatic factors, paving the way for the development of more resistant and durable packaging materials in the face of variable environmental conditions.Highlights The objective of this study is to analyze and describe the effects of natural weathering on high‐density polyethylene bottles. This involves evaluating the deterioration of physicochemical, mechanical, and morphological properties. Additionally, three damage laws are employed to assess the extent of damage inflicted by this material. Analytical techniques were used, including SEM, FTIR, and TGA, tensile and compressive test.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.