Abstract

The purpose of this study was to evaluate the effect of primers on bonding between a silver-palladium-copper-gold alloy and an indirect composite material. Cast disks were air-abraded with alumina, conditioned with one of five primers (Alloy Primer, Luna-Wing Primer, Metal Primer II, Metaltite, M.L. Primer), and bonded with a light-activated indirect composite. Shear bond strengths were determined after 20,000 times of thermocycling. The results showed that four of the primers, except the Luna-Wing Primer, were effective in enhancing the bond strength as compared with the unprimed control group. Of these four primers, Alloy Primer, Metal Primer II, and M.L. Primer exhibited significantly greater bond strengths. It can be concluded that the effectiveness of primers varies considerably according to the organic sulfur compounds added to the solvent, and that care must be taken in selecting priming agents for bonding the composite material and the silver-palladium-copper-gold alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.