Abstract

In this study, the fatigue fracture criterion of the adhesively bonded joint is discussed. The singular stress field is formed at the interface end in the butt joint and causes the debonding fracture. The singular stress field is represented with the intensity of singular stress field (ISSF). The static debonding strength of the adhesively bonded joints is expressed with a constant value of critical ISSF. The rotating-bending fatigue tests are carried out on the butt joints of 15mm in diameter with four different adhesive thicknesses of 109 - 159μm, 209 - 265μm, 393 - 432μm and 754 - 841μm. The evaluation method by the ISSF is applied to the experimental results. It is found that the fatigue strength of the butt joint can be expressed with the constant value of critical ISSF.