Abstract

A method to estimate the electrochemical active site density (SD) of carbon (C) and nitrogen-doped carbon (N/C-900) using phosphomolybdate (PMo12) as a probe molecule is proposed. The complete coverage of the active sites by the probe molecules is established irrespective of the adsorbate concentration (1, 5, or 10 mM), potential cycling (1 or 10 cycles) and cleaning time (2, 5, or 10 min). A conversion factor derived from a smooth and polished glassy carbon disk of known geometrical area is used to estimate the electrochemical active surface area (ECSA) of the carbon catalyst from the SD. The relatively higher SD values estimated from DC voltammetry than from large-amplitude Fourier-transform alternating-current voltammetry (FTacV) is indicative of the contribution of capacitive charge in the former. Adsorbed probe molecules (PMo12) can readily be desorbed from the catalyst surface by cycling the electrode to lower potentials. The active site density of N/C-900 (∼0.36 × 1019 sites g-1) is higher than that of C (∼0.17 × 1019 sites g-1).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.