Abstract

In order to enhance the visible-light transmittance while reducing the insulator–metal transition (IMT) temperature, Hf–W co-doping is designed for modification of VO2. We grow high-quality HfxWyV1−x−yO2 (HfWVO2) alloy films on c-plane sapphire substrates by pulsed laser deposition, and test structural, electrical, and optical properties of the films by various techniques. The Hf–W co-doped VO2 films exhibit outstanding thermochromic performances with a high luminous transmittance up to 41.1%, a fairly good near-infrared modulation capacity of 13.1%, and a low phase transition temperature of 38.9 °C. The enhanced luminous transmittance along with reduced IMT temperature in HfWVO2 is attributed to the co-doping synergetic effect of Hf and W, which effectively improves the optical bandgap and donates extra electrons into the system, respectively, while largely retaining the near-infrared modulation capacity of VO2. Our work provides an effective strategy in tailoring VO2 toward practical smart-coating applications by Hf–W co-doping.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.