2% Al-doped ZnO (AZO) thin films fabricated at 300 °C by pulsed laser deposition (PLD) on amorphous fused silica demonstrated the high quality crystallinity and grain connection, which correlates to the high thermoelectric performance: electrical conductivity σ = 923 S/cm and Seebeck coefficient S = −111 µV/K at 600 K. Its power factor (S2 · σ) is 1.2 × 10−3 W m−1 K−2, twofold better than films deposited on crystalline SrTiO3 under the same experimental conditions. Using our measured thermal conductivity (κ) at 300 K (4.89 W m−1 K−1), the figure of merit, ZT = (S2 · σ · T/κ), is calculated as 0.045 at 600 K, 5 times larger than ZT of our previously reported bulk ZnO.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.