Abstract

The fatigue properties are critical considerations for porous structures, and most of the existing porous materials have unsatisfactory performances due to a lack of structural optimization. This work shows that a topology-optimized structure fabricated by selective laser melting using commercial-purity titanium (CP-Ti) exhibits excellent fatigue properties with an ultra-high normalized fatigue life of ∼0.65 at 106 cycles and at a low density of 1.3 g/cm3. The main factors affecting fatigue, i.e., material properties and a porous structure were studied. Both the factors can affect the fatigue crack initiation time, thereby affecting the fatigue life. Because of twinning that occurred during the fatigue process, the porous CP-Ti samples exhibit a high plasticity. In addition, the fatigue crack propagation rate is significantly reduced because of the high plasticity of the CP-Ti material and the occurrence of fatigue crack deflection.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.