Abstract

The value of electro-optic coefficient r33 of an electro-optic (EO) polymer film depends on the polarization density achieved after the electric poling process. In this letter, we report a high temperature liquid contact poling method which provides a poling field as high as 250 V/μm in LD-3 EO polymer film with less surface damages. The r33 value was measured to be 18 pm/V at 633 nm which is 40°/V higher than the previous reported datum. Such a high poling field and therefore larger r33 value are not achievable through either contact poling or corona poling.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.