Lead-free piezoceramics (K0.5N0.5)NbO3-x wt% Bi4Ti3O12 were fabricated, and effects of Bi4Ti3O12 on the properties of (K0.5N0.5)NbO3 ceramics were investigated. The results show that the orthorhombic and tetragonal transition temperature of the ceramics shifts toward room temperature and a small amount of Bi4Ti3O12 cannot influence the symmetry of (K0.5N0.5)NbO3 ceramics but improve their electrical properties. Optimum piezoelectric properties are owned by (K0.5N0.5)NbO3–0.50 wt% Bi4Ti3O12: d 33 = 135 pC/N, k p = 36.4%, and T C = 406°C, whereas the relatively superb ferroelectric properties are obtained by (K0.5N0.5)NbO3–0.75 wt% Bi4Ti3O12: P r = 27.2 μC/cm2, E c = 7.6 kV/cm, and T C = 398°C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.