Abstract

The microstructure and soft magnetic properties under direct current (DC) mode and alternating current (AC) mode of FeCoNiAl1−xSix (x = 0.2, 0.4, 0.6) high-entropy alloys (HEAs) are investigated. All the studied HEAs show body-centered cubic (BCC) structures, and the [100] texture is formed in the x = 0.4 HEA. The iron (Fe) segregation at the grain boundaries is helpful in increasing the soft magnetic properties under DC. The FeCoNiAl0.6Si0.4 (x = 0.4) HEA exhibits optimal DC and AC soft magnetic properties, primarily due to the formation of the texture along the easy magnetization axis. The x = 0.4 HEA shows the highest permeability (μi = 344 and μm = 1334) and the smallest coercivity (Hc = 51 A/m), remanence (Br = 132 mT), and hysteresis loss (Pu = 205 J/m3). In comparison to the x = 0.2 HEA and x = 0.6 HEA, the total loss (AC Ps) at 50 Hz of the x = 0.4 HEA is decreased by 15% and 18%, and it is reduced at 950 Hz by 13% and 7%. Our findings can provide a useful approach for developing novel HEAs with increased soft magnetic properties by tuning ferromagnetic elemental segregation and forming the texture along the easy magnetization axis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.