Abstract
As a high energy density cathode material, further development of high working voltage spinel LiNi0.5Mn1.5O4 has hindered by its rapid capacity degradation. To address this, a hetero-valent substitution of magnesium for manganese was used to synthesize spinel LiNi0.5MgxMn1.5-xO4 (x = 0, 0.03, 0.05) via a microwave sol-gel method. XRD and refined results indicate that such strategy leads to the modification of the 16c interstitial sites. The electrical performance demonstrates that a modest substitution (x = 0.03) significantly improves both rate performance (113.1 mAh/g, charge and discharge at 5 C) and cycling stability (85% capacity retention after 500 cycles at 1 C). A higher substitution level (x = 0.05) markedly improves high-rate cycling performance, achieving 96% capacity retention after 500 cycles at 5 C. It offers tailored solutions for various application needs, including capacity-focused and high-current-rate applications. Furthermore, the stable LiNi0.5Mg0.05Mn1.45O4 sample could also serve as an effective coating layer for other electrode materials to enhance their cycling stability.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have