Abstract
Spinel LiMn2O4 particles were successfully coated with CuO, MgO, ZnO, Al2O3 and CeO2 by a melting impregnation method. Except for the CeO2-coated sample, all the others exhibit better cycling stability than bare LiMn2O4 at room temperature and at 55°C. Among these samples, the ZnO-coated sample shows the best cycling stability. A capacity of 100 mA·h·g−1 still remained after 100 cycles at 55°C while the bare LiMn2O4 retains a capacity of only 80 mA·h·g−1 after the same number of cycles. The improvement in the cycling stability is attributed to the suppressed Mn dissolution caused by HF.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.