Abstract
A series of controllable emissions SrWO4 :Eu3+ and charge-compensated SrWO4 : Eum3+ (m=0.01 or 0.20) phosphors was successfully prepared via a simple co-precipitation method. The energy transfer mechanism was studied based on the Huang's theory. A low magnitude of Huang-Rhys factor (10-2 ) was calculated using phonon sideband spectra. The Judd-Ofelt parameters Ωλ (λ=2, 4 and 6) of Eu3+ -activated SrWO4 doped with charge compensation were obtained. The calculated Commission Internationale de l'Eclairage chromaticity coordinates were found to be about (0.67, 0.33) for SrWO4 : Eu0.203+ and charge-compensated SrWO4 : Eu0.203+ phosphors, which coincided with the National Television Standard Committee system standard values for red. A white light emission was obtained under 362nm excitation. The correlated color temperature was computed by a simple equation to characterize light sources. Thus, warm white light-emitting diodes with higher Ra can be constructed by combining as-prepared high efficiency, low correlated color temperature and high color purity phosphor.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.