Abstract

The influence of emitter surface morphology on emission site density (ESD) is investigated for carbon nanotube films. The authors show that the ESD varies with cathode-anode distance for rough surface emitters while it is almost invariant for smooth ones. In addition, it has been revealed that the ESD decreases with the increase in the film area, resulting in low emission current density for large-area films. The present study suggests that the high ESD is more important to achieve high emission current density and long lifetime for film emitters than the high field enhancement factor.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.