AbstractUltrafine polystyrene (PS)/poly(2‐methoxy‐5‐(2′‐ethylhexyloxy)‐1,4‐phenylene vinylene) (MEH‐PPV) fibers were successfully prepared by electrospinning of PS/MEH‐PPV solutions in chloroform, 1,2‐dichloroethane, and tetrahydrofuran (THF). Three concentrations of the solutions were prepared: 8.5, 16, and 23.5% (w/v), with the compositional weight ratios between PS and MEH‐PPV being 7.5:1, 15:1, and 22.5:1, respectively. Smooth fibers only observed from 23.5% (w/v) PS/MEH‐PPV solution in chloroform. Improvement in the electrospinnability of 8.5% (w/v) PS/MEH‐PPV solution in chloroform was achieved by addition of an organic salt, pyridinium formate (PF), or by addition of a minor solvent with a high dielectric constant value. The average diameters of the as‐spun PS/MEH‐PPV fibers were between 0.30 and 5.11 μm. Last, photoluminescence of 8.5% (w/v) solutions of PS/MEH‐PPV in a mixed solvent system of chloroform and 1,2‐dichloroethane of various volumetric compositions and the resulting as‐spun fibers was investigated and compared. © 2005 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 43: 1881–1891, 2005

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.