Measurements of the electrical resistivity, rho , and thermopower S, of high-purity liquid Ca and Sr are reported. It is found that, at the melting temperature, rho =23.0, S=15.2, and (1/ rho )(d rho /dT)=+6.1 for Ca, and rho =87.0, S=0.3, and (1/ rho )(d rho /dT)=-0.46 for Sr, where the units are mu Omega cm, mu V degrees C-1, and degrees C-1, and degrees C-1, respectively. These values are compared with recent calculations, special attention being given to the unusually large and positive value of (1/ rho )(d rho /dT) for Ca.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.