Abstract

Measurements of electrical resistivity, rho , and thermopower, S, of solid (above room temperature) and liquid high-purity Eu and Yb are reported. No evidence for the suggested 'transition' in solid Yb at about 300 degrees C is seen in either rho (T) or S(T). Measured values for rho , d rho /dT, and S for these liquid metals at their melting temperatures are, respectively, 241, -0.066, and 6.6 (for EU), and 113.8, -0.023, and -12.2 (for Yb), where the units are mu Omega cm, mu Omega cm degrees C-1, and mu V degrees C-1, respectively. These liquid values are compared with recent calculations based on the t matrix.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.