Abstract

Abstract A spent tanning bath contains high concentration of salts, chromium and protein. The treatment system for removal of chlorides or chromium from this effluent is expensive. In this context this waste has to be reused. Our study focuses on the application of advanced oxidation processes for protein removal present in a tanning bath. To improve the quality of the chromium tanning bath, two electrochemical processes (electrooxidation and peroxi-electrocoagulation process, PEP) are investigated in a batch reactor. The effects of operational parameters such as reactor configuration, current density and electrolysis time on chemical oxygen demand (COD) and protein removal efficiency are examined. Results indicated that under the optimum operating range for process, the COD and protein removal efficiency reached 53 and 100%, respectively. The optimum values are determined for the hybrid process (PEP) under 0.13 A·cm−2 over 2 h. The treated tanning bath is used as a tanning solution in leather processing. The influence of chromium salt dose, pH solution, stirring time and contact time on the leather characteristic is evaluated. The hides tanned after the addition of 0.25% of commercial chromium salt, at pH solution, leaving them stirring for 4 h with a contact time of 2 days, and showed good hydrothermal stability and physical characteristics of leather.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.