Abstract

This paper is aimed at identifying the different mechanisms of hydrogen bubble evolution on Pt disk electrodes of different sizes (0.5, 1.0, and 5.0 mm in diam) in a wide current density range. This was accomplished by means of time and frequency electrochemical noise analysis combining potential and electrolyte resistance fluctuations simultaneously measured to separate ohmic and nonohmic fluctuations. At weak current densities, coalescence processes were shown to be a major component of bubble growth in the case of small electrodes while diffusion-controlled bubble growth was dominant on larger surface ones. For all electrode diameters, a new mechanism was spontaneously switched on at higher current densities to enhance evacuation of dissolved gas produced at the interface. This new mechanism was a periodical gas-oscillator collective phenomenon originated in the simultaneous evolution of bubbles at the border of the electrode where the metal-insulator discontinuity acted as a continuous gas cavity, giving preferential bubble nucleation. Once present, the gas-oscillator mechanism was a strongly dominant component of the evolution process, so that most of the bubble production was shifted from the center to the edge of the electrode. © 2002 The Electrochemical Society. All rights reserved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.