Abstract

In order to evaluate the potential of the new light-weight structural TiAl alloy for marine application, the electrochemical corrosion and tribological behavior of TiAl alloy in a sea water environment have been investigated in this paper. A commercial Al 5083 marine product was selected as the control tests. The counterface materials include SiC, GCr15 steel and Hastelloy C276 alloy. TiAl alloy exhibits excellent corrosion resistance over Al 5083 alloy in sea water. The wear behavior of the two materials in sea water is sensitive to counterface materials. With GCr15 steel and C276 alloy as the mating surfaces, the wear resistance of TiAl alloy is significantly superior to that of Al 5083 alloy in sea water.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.