Abstract
Polypropylene (PP) composite materials with both high mechanical toughness and electrical insulation performance are prepared by incorporating styrene-ethylene/butylene-styrene (SEBS) block copolymer as a toughening agent and nanoscale silica (SiO2) as a inorganic modifier to enhance electrical-tree and breakdown resistances. The effects and mechanisms of SEBS toughening agent and SiO2 nanofiller on the thermal-mechanical properties and electrical insulation performances of PP material are investigated through the mechanical tests as well as the accelerated electrical-tree aging and alternative current (AC) breakdown experiments. The elastic modulus of SiO2/SEBS/PP composite is slightly lower than that of pure PP material, while the thermal elongation rate remains superior to cross-linked polyethylene (XLPE), which is competent in mechanical performances for main insulation materials in high-voltage cables. The addition of styrene-ethylene/butylene-styrene (SEBS) facilitates electrical-tree growth in PP matrix and thus leads to the reduction in dielectric breakdown strength of PP material. In contrast, the incorporation of nano-SiO2 can effectively improve the electrical-tree resistance and dielectric breakdown strength of PP material, making the SiO2/SEBS/PP composite a promising candidate for high-voltage cable insulation. The tests and analyses of thermal stimulated depolarization current (TSDC) reveal that the SEBS toughing additive introduces the shallow charge traps in PP matrix, making it easier for the trapped charges to transition into charge carriers, thus leading to a considerable decrease in electrical-tree resistance and insulation strength of PP material. Meanwhile, the SiO2 nanofiller can introduce deeper charge traps into PP matrix than the structural-defect intrinsic charge traps, resulting in a significant amelioration in the electrical-tree resistant and insulation performances for SEBS/PP composite. The present study demonstrates that SiO2/SEBS/PP composite possesses sufficiently high electrical-tree resistance and dielectric breakdown strength as well as suitable thermal-mechanical properties, offering a potential application in main insulation of high-voltage cables and providing an effective pathway for developing novel recyclable AC high-voltage cables.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.