Abstract
We report on the properties of photovoltaic (PV) structures based on thin films of n-type zinc oxide grown by atomic layer deposition method on a cheap silicon substrate. Thin films of ZnO are used as n-type partner to p-type Si (110) and, when doped with Al, as a transparent electrode. PV structures with different thicknesses of ZnO layers (from 600 nm to 1600 nm) were deposited to determine the optimal performance of PV structures. The best response we obtained for the structure with ZnO layer thickness of 800 nm. The so-obtained PV structures show 6% efficiency.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.