Abstract

The adiabatic elastic constants were determined for niobium and niobium-molybdenum alloys of the following nominal compositions: 15, 25, 35, 50, 75, and 90 wt.% Mo. The c11, c12, and c44 elastic constants of these bcc alloys were tabulated between −190 and +100°C. The effects of compositional changes on the elastic constants were far greater than those due to temperature. An anomalous temperature dependence for c44 was found for the niobium-rich alloys. An analysis of the elastic constants in terms of central forces revealed that nearest-and second-nearest-neighbor force constants rise with molybdenum additions, with the latter tending towards a maximum as the composition of pure molybdenum is approached. This is thought to be associated with the filling of a d subband. The Debye temperatures were computed and found to be generally in good agreement with the calorimetrically determined values reported in the literature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.