Abstract
Cavitation damage tests in various polymer solutions have been carried out using a vibratory damage apparatus. The relation of weight loss-time, the damage patterns, the cavitation clouds and the damaged area in a polyacrylamide solution, a sodium carboxy-methylcellulose solution, a hydroxyethylcellulose solution, a guar gum solution and a polyethylene oxide solution are compared and are discussed. It is found that the weight losses in the PAM solution and the Polyox solution, which are more elastic, are smaller than the cases of the other polymer solutions and water after sixty minutes exposure to cavitation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.