Abstract

Phosphoric acid-activated geopolymer (PAG) is an environmentally friendly cementing material with broad application prospects in many fields. Currently, phosphoric acid-activated metakaolin geopolymer (PAMG) is the focus of extensive research. Most studies mainly focus on the effects of metakaolin (MK) activity, phosphoric acid (PA) concentration, mix proportion, and curing system on the compressive strength of PAMG. However, the investigation of additives is extremely limited. In this study, the effects of magnesia and borax on the mechanical properties and microstructure of PAMG were investigated. The compressive strength of PAMG reached 84.31 MPa, indicating a 57.71% increase when the magnesia content was 6%. This increase was attributed to the ability of magnesia to improve the polymerization reaction and gel formation. Furthermore, the addition of 1% borax led to a compressive strength of 87.92 MPa, representing a 64.46% improvement. The presence of borax facilitated gel formation and enhanced the gel structure through the BO bond.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.