Abstract

Effects of a small amount addition of Cr on glass-forming ability (GFA) and mechanical properties of Cu–Zr–Al bulk metallic glass were investigated. The GFA of (Cu46Zr46Al8)100−x Cr x (x = 0, 0.25, 0.5, 0.75, and 1 at%) alloys tends to decrease with the increasing Cr content. A good correlation between the GFA and the temperature interval of supercooled liquid region ΔT x or parameter γ exists in these alloys. Addition of an appropriate amount of Cr can significantly improve the plasticity of the alloys. The bulk metallic glass with x = 0.5 exhibits promising mechanical properties with high fracture strength of 1870 MPa and obvious plastic strain of 2.23%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.