The purpose of the present study was to evaluate the bond strength and durability of four bonding systems joined to a prefabricated porcelain material (Vita Celay Blanks). Two sizes of porcelain block were bonded with one of the following systems: (1) Clapearl Bonding Agent and Clapearl DC; (2) Imperva Porcelain Primer and Imperva Dual; (3) Monobond S and Variolink II; or (4) Tokuso Ceramics Primer and Bistite II. Shear bond strength was measured after 24-hour immersion in water and after subsequent thermocycling. The average pre- and post-thermocycling bond strengths in MPa (n=8) were: 52.5 and 42.5 for bonding system (1), 47.7 and 32.8 for (2), 55.0 and 48.8 for (3), and 51.5 and 25.6 for (4). Although prethermocycling results were not statistically different from each other, Group (3) exhibited the greatest strength after thermocycling.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.