Abstract

Highly crystalline ZnO nanoparticles (NPs) were synthesized with zinc acetate as precursor and oxalic acid at 80°C through the simple solution phase approach. The synthesized ZnO NPs possessed monodispersity with the average size 20–30nm. The crystalline properties revealed the typical hexagonal wurtzite phase with orientation along c-axis. The photocatalytic activity investigation was carried out by performing the decomposition of rhodamine-B dye under UV illumination over as-synthesized ZnO NPs. The rhodamine B dye considerably degraded by ∼95% within 70min in the presence of as-synthesized ZnO NPs. An excellent rate constant (k=0.0343min−1) was obtained for the degradation of rhodamine B dye.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.