Abstract
AA6082-T6 alloy was joined by friction stir spot welding using five different pin profiles, namely cylindrical, conical, triangular, hexagonal, and cylindrical with two grooves, at different dwell time. The joints welded by cylindrical pins had larger effective weld width. However, grooves on the cylindrical pin decreased the effective weld width. In the weld made with the hexagonal pin, the hook was bent downward from the interface of the sheets and had the smallest effective weld width. When the conical pin was used, the effective weld width increased with increasing dwell time. In the case of using tools with cylindrical and conical pins, HAZ hardness was relatively lower. With increasing dwell time, HAZ hardness of the joints made with the conical pin decreased. Effective weld width determined the weld strength under the tensile shear loading condition: larger effective weld width resulted in higher weld strength. Weld strength of the joints made with cylindrical pins was higher. The joints fabricated with hexagonal pins had the lowest weld strength. In general, higher dwell time led to higher weld strength. The welds with the higher strength experienced both brittle and ductile fractures, while the joints with the lower strength exhibited completely brittle fracture.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of the Canadian Society for Mechanical Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.