208 mm diameter single crystals are grown by Czochralski method with different growing conditions, and the effects of the ingot cooling on point defect behavior and the shape of the crystal–melt interface are experimentally investigated. In order to obtain various cooling rates of the ingot, cooling-water jacket is changed with various surface conditions, which are different emissivities of the material, and various melt gaps are applied in the experiments, where melt gap is defined as the distance from heat shield to the melt free-surface. The crystal–melt interface becomes more concave (convex to the crystal) and the critical pulling speed for defect-free crystal increases with increasing cooling rate of the ingot.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.